Advanced cast iron processes (induction furnace, AI-controlled alloy design) demand high-performance carburizers for optimal carbon recovery. Key considerations:
Selection Criteria:
Fixed carbon ≥98.5%, sulfur ≤0.03% (minimize slag inclusion)
1-5mm granularity (uniform dissolution)
Graphitized petroleum coke preferred (20% higher efficiency)
Usage Protocols:
Add in batches at 1400-1500℃ (avoid direct high-temperature exposure)
Mix thoroughly with scrap steel
Store in dry, dark conditions; use within 72hrs after opening